    The Electromechanical Creep Testing Machine KAPPA DS offers a wide range of applications.
    • Creep tests
    • Creep rupture tests
    • Stress rupture tests
    • Relaxation tests
    • Creep crack tests
    • Definition of individual stepless sequences of load and temperature
    • ‘Advanced creep‘ – Tests
    – Creep fatigue tests
    – Creep strain modelling (e.g. to give creep strength at various levels of strain)
    – Creep ductility
    – Creep property deterioration due to serviceexposure
    – Creep data from component tests
    • Additional load-, stress- and strain-controlled tests such as tensile, compression, flexure,

    More Detail

  • KAPPA LA Zwick/Roell

    Application
    • Creep tests
    • Creep rupture tests
    • Stress rupture tests
    • Relaxation tests (only with spring loaded system)
    • Creep crack tests
    • Definition of individual stepless sequences of temperature
    • Ambient or elevated temperature
    • For long term tests (reaching more than 10.000h